A 235 400-520 22 ≤0.21 ≥2.5 ≤0.5 ≤0.035 ≤0.035
B ≤0.21 ≥0.80 ≤0.35
D ≤0.21 ≥0.60 ≤0.35
E ≤0.18 ≥0.70 ≤0.35
高强度船体结构钢力学性能与化学成份
钢材级别 屈服点σs
(MPa)不小于 抗拉强度
σb(MPa) 伸长率σ%
不小于 碳
C 锰
Mn 硅
Si 硫
S 磷
P
A32 315 440-570 22 ≤0.18 ≥0.9-1.60 ≤0.50 ≤0.035 ≤0.035
D32
E32
F32 ≤0.16 ≤0.025 ≤0.025
A36 355 490-630 21 ≤0.18 ≤0.035 ≤0.035
D36
E36
F36 ≤0.16 ≤0.025 ≤0.025
A40 390 510-660 20 ≤0.18 ≤0.035 ≤0.035
D40
E40